[1. Schotte, B. A study of electrolytic reduction of corroded lead objects and application, characterization and testing of a protective lead carboxylate coating. Disertační práce, Universiteit Gent: Faculty of Science, 2007.]Search in Google Scholar
[2. Selwyn, L.; et al. Lead (Pb). In Metals and Corrosion: A Handbook for the Conservation Professional. 1st ed.; Canadian Conservation Institute: Canada, 2004; pp 115–123. ISBN 0-662-37984-5.]Search in Google Scholar
[3. Kolektiv autorů. Konzervování a restaurování olova a jeho slitin. In Konzervování a restaurování kovů. 1st ed.; Technické muzeum v Brně: Brno, 2011; pp 526-544. ISBN 978-80-86413-70-9]Search in Google Scholar
[4. Costa, V. Electrochemistry as a conservation tool: an overview. Conservation Science, 2003, 88-95.]Search in Google Scholar
[5. Jareš, V. Metalografie neželezných kovů. 1st ed.; Nakladatelství ČSAV: Praha, 1950.]Search in Google Scholar
[6. Vojtěch, D. Olovo a jeho slitiny. In Materiály a jejich mezní stavy. 1st ed.; VŠCHT: Praha, 2010; pp 35–36. ISBN 978-80-7080-741-5.]Search in Google Scholar
[7. Kratochvíl, B.; Švorčík, V.; Vojtěch, D. Slitiny neželezných kovů. In Úvod do studia materiálů. 1st ed.; VŠCHT: Praha, 2005; pp 164–165. ISBN 80-7080-568-4.]Search in Google Scholar
[8. Costa,V.; Urban, F. Lead and its alloys: metallurgy, deterioration and conservation. Reviews in Conservation2005, 6, 48–62.10.1179/sic.2005.50.Supplement-1.48]Search in Google Scholar
[9. Schotte, B.; Adriens, A. The treatment of corroded lead artefacts. Studies in Conservation2006, 51, 1–8.]Search in Google Scholar
[10. Lyon, S. B. Corrosion of Lead and its Alloys. Corrosion and Protection Center. University of Manchester: Manchester, 2010.10.1016/B978-044452787-5.00098-6]Search in Google Scholar
[11. Leygraf, C.; Graedel, T. E. Atmospheric Corrosion of Lead. In Atmospheric Corrosion, 1st ed.; Canada, 2000; pp 295–304. ISBN 0-471-37219-6.]Search in Google Scholar
[12. Niklasson, A.; Johansson, L.; Svensson, J. The influence of relative humidity and temperature on the acetic acid vapour-induced atmospheric corrosion of lead. Corrosion Science2008, 50, 3031–3037.10.1016/j.corsci.2008.08.009]Search in Google Scholar
[13. Ryhl-Svendsen, M. Corrosivity measurements of indoor museum environments using lead coupons as dosimeters. Journal of Cultural Heritage2008, 9, 285–293.10.1016/j.culher.2008.01.005]Search in Google Scholar
[14. Angeliny, E.; Grassini, S.: Underwater corrosion of metallic heritage artefacts. In Corrosion and conservation of cultural heritage metallic artefacts, 1st ed.; Woodhead Publishing Limited: Oxford, 2013; pp 236–259.10.1533/9781782421573.3.236]Search in Google Scholar
[15. Grayburn, R.; et al. Time-lapse synchrotron X-ray diffraction to monitor conservation coatings for heritage lead in atmospheres polluted with oak-emitted volatile organic compounds. Corrosion Science2014, 82, 280–289.10.1016/j.corsci.2014.01.027]Search in Google Scholar
[16. Sastri, V. S. Vapor phase corrosion inhibitors. In Corrosion Inhibitors Principles and Aplications, 1st ed.; John Wiley and Sons Ltd: Chichester, 1998, pp 787–822.]Search in Google Scholar
[17. Guidelines for the Storage and Display of Archaeological Metalwork [Online]. Engish heritage, 2013, pp 12-13. http://www.english-heritage.org.uk/content/learn/conservation/2543455/2543024/guidelines-for-the-storage-and-display-of-archaeological-metalwork.pdf (accessed 11 Jan 2019)]Search in Google Scholar
[18. Ďurovič, M.; et al. Restaurování a konzervování archiválií a knih, 1st ed.; Paseka: Praha, 2002. ISBN 80-7185-383-6.]Search in Google Scholar
[19. Vávrová, P. Koroze a degradace papíru. Koroze a degradace materiálu. http://www.vscht.cz/met/stranky/vyuka/predmety/koroze_materialu_pro_restauratory/kadm/pdf/1_3.pdf (accessed 11 Jan 2019).]Search in Google Scholar
[20. Proniewicz, L. M.; Paluszkiewicz, C.; Weselucha-Birczynska, A.; Baranski, A.; Dutka, D. FT-IR and FT-Raman study of hydrothermally degraded groundwood containing paper. Journal of Molecular Structure2002, 614, 345–353.10.1016/S0022-2860(02)00275-2]Search in Google Scholar
[21. Ďurovič, M. Vlastnosti papíru a jeho degradace. http://www.vscht.cz/met/stranky/vyuka/labcv/labor/res_vlastnosti_papiru/teorie.htm (accessed 11 Jan 2019).]Search in Google Scholar
[22. Hatchfield, B. P. Pollutants in the Museum Environment; Archetype Publications: London, 2002. ISBN 1-873132-96-4.]Search in Google Scholar
[23. Gibson, L. T.; Watt, C. M. Acetic and formic acids emitted from wood samples and their effect on selected materials in museum environments. Corrosion Science 2010, 52, 172–178.10.1016/j.corsci.2009.08.054]Search in Google Scholar
[24. Coles, E. L.; Gibson J. G.; Hinde, R. M.: The corrosion of lead by dilute aqueous organic acids, Journal of Applied Chemistry1958, 341-348.10.1002/jctb.5010080511]Search in Google Scholar
[25. Schotte, B.; Adriens, A. The treatment of corroded lead artefacts. Studies in Conservation2006, 51, 1–8.10.1179/sic.2006.51.4.297]Search in Google Scholar
[26. Turgoose, S. The corrosion of lead and tin: before and after excavation. In Lead and Tin Studies in Conservation and Technology, United Kingdom Institute for Conservation: London, 1985, pp 15–23.]Search in Google Scholar
[27. Niklasson, A.; Johansson, L.; Svensson, J. Atmospheric corrosion of historical organ pipes´influence of acetic and formic acid vapour and water leaching on lead. Proceedings of Metal 2004, 179–273.]Search in Google Scholar
[28. Stambolov, T. The Corrosion and Conservation of Metallic Antiquities and Works of Arts. Central research laboratory of objects of art and science: Amsterdam, 1985, pp 160-173.]Search in Google Scholar
[29. Nejedlý, V. Restaurování sochy Atlanta z astronomické věže pražského Klementina, Zprávy památkové péče LVII 1997, 2, 46-49.]Search in Google Scholar
[30. Caley, E. Coatings and incrustations on lead objects from the agora and the method used for their removal. Studies in Conservation1955, 2, 49–54.10.1179/sic.1955.007]Search in Google Scholar
[31. Organ, R. Use of ion-exchange resin in the treatment of lead objects. Museums Journal1953, 53, 49–52.]Search in Google Scholar
[32. Škeřík, J. Receptář pro elektrotechnika. 3rd ed. Státní nakladatelství technické literatury: Praha, 1982.]Search in Google Scholar
[33. Fawzy, M. A., et al. Corrosion behaviour of Pb-Sn binary alloys in acid solutions. Surface and Coatings Technology1981, 14, 257–264.10.1016/0376-4583(81)90088-1]Search in Google Scholar
[34. Rocca, E., et al. Inhibition treatment of the corrosion of lead artefacts in atmospheric conditions and by acetic acid vapour: use of sodium decanoate. Corrosion Science2004, 46, 653-665.10.1016/S0010-938X(03)00175-6]Search in Google Scholar
[35. Cano, E.; Lafuente, D. Corrosion inhibitors for the preservation of metallic heritage artefacts. In Corrosion and conservation of cultural heritage metallic artefacts, 1st ed.; Woodhead Publishing Limited: Oxford, 2013, pp 570–594.10.1533/9781782421573.5.570]Search in Google Scholar
[36. Sankarapapavinasam, S., et al. Hydrazine and substituted hydrazines as corrosion inhibitors for lead in acetic acid. British Corrosion Journal1989, 24 (1), 39-42.10.1179/000705989798270351]Search in Google Scholar
[37. Chiavari, C.; Martiny, C. Conservation of organ pipes: protective treatments of lead exposed to acetic acid vapours. In Metal 04, Proceedings of the International Conference on Metals Conservation, Canberra, October 4-8, 2004, National Museum of Australia: Canberra, 2004, pp 281-293.]Search in Google Scholar
[38. Rocca, E.; Steinmetz, J. Inhibition of lead corrosion with saturated linear aliphatic chain monocarboxylates of sodium, Corrosion Science2001, 43, 891-902.10.1016/S0010-938X(00)00115-3]Search in Google Scholar
[39. Inhibitory koroze kovů. http://ukmki.vscht.cz/files/uzel/0016736/Inhibitory%20koroze%20kov%C5%AF.pdf ? redirected (accessed 11 Jan 2019)]Search in Google Scholar
[40. Lacouture, F.; Francois, M.; Didierjean, C.; Rivera, J. P.; Rocca, E.; Steinmetz, J. Anhydrous lead(II) heptanoate. Acta Crystallogr.2001, 57, 530–531.10.1107/S0108270101001615]Search in Google Scholar
[41. Green, L. A re-evaluation of lead conservation techniques at the British museum. International Restorer Seminar, Veszprém, Hungary, July 1-10, 1989.]Search in Google Scholar
[42. De Keersmacker, M.; De Wael, K.; Adriaens, A.: Influence of the deposition method, temperature and deposition time on the corrosion inhibition of lead dodecanoate coatings deposited on lead surfaces. Journal of Solid State Electrochemistry2013, 17, 1259–1270.10.1007/s10008-012-1964-4]Search in Google Scholar
[43. Pecenová, Z.; Kouřil, M. Ochrana historického olova proti parám kyseliny octové. Koroze a ochrana materiálu2016, 60(1), 28-34.10.1515/kom-2016-0002]Search in Google Scholar
[44. Adriens, A.; De Bisshop, F.; et al. Growth and real time corrosion resistance monitoring of lead decanoate coatings. Applied Surface Scince2008, 254, 7351–7355.10.1016/j.apsusc.2008.05.333]Search in Google Scholar
[45. Kouril, M.; Prosek, T.; Scheffel, B.; Degres, Y. Corrosion monitoring in archives by the electrical resistance technique. Journal of Cultural Heritage2014, 15(2), 99-103.10.1016/j.culher.2013.04.002]Search in Google Scholar
[46. Kouril, M.; Prosek, T.; Scheffel, B.; Dubois, F. High sensitivity electrical resistance sensors for indoor corrosion monitoring. Corrosion Engineering, Science and Technology2013, 48(4), 282-287.10.1179/1743278212Y.0000000074]Search in Google Scholar
[47. Prosek, T.; Kouril, M.; Dubus, M.; Taube, M.; Hubert, V.; Scheffel, B.; Degres, Y.; Jouannic, M.; Thierry, D. Real-time monitoring of indoor air corrosivity in cultural heritage institutions with metallic electrical resistance sensors. Studies in Conservation2013, 58(2), 117-128.10.1179/2047058412Y.0000000080]Search in Google Scholar