DBSA doped polypyrrole blended with Poly(4-styrenesulfonic acid) by mechanical mixing
, , , , , oraz
19 gru 2014
O artykule
Data publikacji: 19 gru 2014
Zakres stron: 648 - 651
DOI: https://doi.org/10.2478/s13536-014-0234-9
Słowa kluczowe
© 2014 Wroclaw University of Technology
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.
DBSA doped polypyrrole was prepared by In-situ chemical oxidative polymerization method. The reaction temperature was 0 to 20 °C. Different weight percentages of PSS (40 wt.%, 60 wt.% and 80 wt.%) were mechanically blended with a pestle in an agate mortar for 25 minutes by solid state mixing. The investigation of the blend focused on the optical, structural and morphological properties. SEM micrographs indicated that PSS was homogeneously distributed within DBSA doped PPy. FT-IR study confirmed the doped and blended dopants in the composite structure. UV-study revealed the π → π* transition in benzenoid rings of DBSA and presence of PSS. The semi-crystalline nature of the composites improved with increasing the weight percentage of PSS.