Accesso libero

Synthesis and solubility of hopeite Zn3(PO4)2·4H2O

,  e   
18 dic 2023
INFORMAZIONI SU QUESTO ARTICOLO

Cita
Scarica la copertina

Figure 1.

XRD pattern of synthetic hopeite.
XRD pattern of synthetic hopeite.

Figure 2.

Scanning electron microscope (SEM) image of synthetic hopeite.
Scanning electron microscope (SEM) image of synthetic hopeite.

Figure 3.

Concentrations of Zn and PO4 in the dissolution experiment with an initial pH of 2.0 (equilibrium pH 4.8) and temperature of 25°C.
Concentrations of Zn and PO4 in the dissolution experiment with an initial pH of 2.0 (equilibrium pH 4.8) and temperature of 25°C.