Accesso libero

The Effect of Long Term Service at Elevated Temperatures on Microstructure Degradation of Austenitic Reformer Tubes

INFORMAZIONI SU QUESTO ARTICOLO

Cita

J. Łabanowski
Gdansk University of Technology, Faculty of Mechanical Engineering, Department of Materials Science and Welding EngineeringGdańsk, Poland
M. Jurkowski
Gdansk University of Technology, Faculty of Mechanical Engineering, Department of Materials Science and Welding EngineeringGdańsk, Poland
M. Landowski
Gdansk University of Technology, Faculty of Mechanical Engineering, Department of Materials Science and Welding EngineeringGdańsk, Poland
eISSN:
2083-4799
Lingua:
Inglese
Frequenza di pubblicazione:
4 volte all'anno
Argomenti della rivista:
Materials Sciences, Functional and Smart Materials