Orthodontic silver brazing alloys suffer from the presence of cadmium, excessive flow temperatures, and crevice corrosion on stainless steel. Seven alloys were examined. Two alloys contained cadmium. The lowest flow temperature observed was 629°C for a cadmium alloy and 651 °C for two cadmium free alloys. Three alloys had corrosion resistance superior to the other solders. Addition of low melting temperature elements gallium and indium reduced flow temperature in some cases but produced brittleness in the brazing alloy.