Production of ZnO and CdO-ZnO thin Films by Extraction–Pyrolytic Method
, , , et
27 juil. 2016
À propos de cet article
Publié en ligne: 27 juil. 2016
Pages: 57 - 66
DOI: https://doi.org/10.1515/lpts-2016-0021
Mots clés
© 2016 A. Cvetkovs et al., published by De Gruyter Open
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.
The extraction-pyrolytic method has been applied to produce the ZnO and CdO-ZnO thin films on glass and quartz glass substrates. According to X-ray diffraction measurements, the ZnO and CdO phases have been produced with an average size of crystallites about 8–42 nm in the films. The thickness of the layers measured by a profilometer has been up to 150 nm. The surface morphology measurements show that the surface of the films may be rough and non-continuous. The SEM results confirm the dependence between the preparation procedure and the quality of the thin film.