DBSA doped polypyrrole blended with Poly(4-styrenesulfonic acid) by mechanical mixing
, , , , , y
19 dic 2014
Acerca de este artículo
Publicado en línea: 19 dic 2014
Páginas: 648 - 651
DOI: https://doi.org/10.2478/s13536-014-0234-9
Palabras clave
© 2014 Wroclaw University of Technology
This work is licensed under the Creative Commons Attribution-NonCommercial-NoDerivatives 3.0 License.
DBSA doped polypyrrole was prepared by In-situ chemical oxidative polymerization method. The reaction temperature was 0 to 20 °C. Different weight percentages of PSS (40 wt.%, 60 wt.% and 80 wt.%) were mechanically blended with a pestle in an agate mortar for 25 minutes by solid state mixing. The investigation of the blend focused on the optical, structural and morphological properties. SEM micrographs indicated that PSS was homogeneously distributed within DBSA doped PPy. FT-IR study confirmed the doped and blended dopants in the composite structure. UV-study revealed the π → π* transition in benzenoid rings of DBSA and presence of PSS. The semi-crystalline nature of the composites improved with increasing the weight percentage of PSS.