Uneingeschränkter Zugang

Rheological Properties of Pullulan and Aloe Vera Nanofiber Solutions

, ,  und   
14. Okt. 2020

Zitieren
COVER HERUNTERLADEN

Figure 1.

The overall process to develop the nanofiber demonstrating the multiple applications.
The overall process to develop the nanofiber demonstrating the multiple applications.

Figure 2.

Nanofiber using PHD 4400 Syringe Pump at 30 kV (a) 10,000 times magnification, (b) 50,000 times magnification
Nanofiber using PHD 4400 Syringe Pump at 30 kV (a) 10,000 times magnification, (b) 50,000 times magnification

Figure 3.

Nanofiber using PHD 4400 Syringe Pump at 28 kV (a) 50,000 times magnification, (b) 25,000 times magnification
Nanofiber using PHD 4400 Syringe Pump at 28 kV (a) 50,000 times magnification, (b) 25,000 times magnification

Figure 4.

Elastic and viscous modulus of a mixture as a function of frequency at 19 oC.
Elastic and viscous modulus of a mixture as a function of frequency at 19 oC.

Figure 5.

Complex modulus as a function of frequency at 19 oC
Complex modulus as a function of frequency at 19 oC

Figure 6.

(a) Viscosity vs. stress, (b) Viscosity vs. shear rate
(a) Viscosity vs. stress, (b) Viscosity vs. shear rate

Figure 7.

Validation of cross model with experimental data.
Validation of cross model with experimental data.

Figure 8.

Storage and loss modulus vs. time
Storage and loss modulus vs. time
Sprache:
Englisch
Zeitrahmen der Veröffentlichung:
4 Hefte pro Jahr
Fachgebiete der Zeitschrift:
Informatik, Informatik, andere