Group Wilcoxon Z DSCF Value p-value
ZirCAD + ZPrime Plus vs. Katana + ZPrime Plus 1.5993 2.2618 0.6828
ZirCAD + ZPrime Plus vs. Cercon + ZPrime Plus 1.2095 1.7105 0.8908
ZirCAD + ZPrime Plus vs. ZirCAD + Monobond -0.3780 0.5345 0.9998
ZirCAD + ZPrime Plus vs. Katana + Monobond 2.2045 3.1177 0.2929
ZirCAD + ZPrime Plus vs. Cercon + Monobond -0.2268 0.3207 1.0000
ZirCAD + ZPrime Plus vs. Comparison -1.0662 1.5079 0.9379
Katana + ZPrime Plus vs. Cercon + ZPrime Plus -0.2666 0.3770 1.0000
Katana + ZPrime Plus vs. ZirCAD + Monobond -2.0436 2.8901 0.3870
Katana + ZPrime Plus vs. Katana + Monobond 1.0585 1.4969 0.9400
Katana + ZPrime Plus vs. Cercon + Monobond -2.3990 3.3927 0.1988
Katana + ZPrime Plus vs. Comparison -1.0502 1.4852 0.9422
Cercon + ZPrime Plus vs. ZirCAD + Monobond -1.2095 1.7105 0.8908
Cercon + ZPrime Plus vs. Katana + Monobond 1.0614 1.5011 0.9392
Cercon + ZPrime Plus vs. Cercon + Monobond -1.6630 2.3519 0.6409
Cercon + ZPrime Plus vs. Comparison -1.0662 1.5079 0.9379
ZirCAD + Monobond vs. Katana + Monobond 1.9596 2.7713 0.4407
ZirCAD + Monobond vs. Cercon + Monobond 0.3024 0.4276 0.9999
ZirCAD + Monobond vs. Comparison -1.0662 1.5079 0.9379
Katana + Monobond vs. Cercon + Monobond -2.6944 3.8105 0.0996
Katana + Monobond vs. Comparison -1.3472 1.9052 0.8296
Cercon + Monobond vs. Comparison -0.8885 1.2566 0.9744

Kruskal-Wallis test.

Chi-Square 11.6391
DF 6
P-value 0.0705

Study products.

Material Composition Manufacturer
Z-Prime Plus Hydroxyethyl methacrylate, BisGMA, methacryloxydecyl dihydrogen phosphate, ethanol Bisco, USA
Monobond Etch & Prime Methacrylated phosphoric acid ester, ethanol Ivoclar Vivadent, USA
Transbond XT Silane Treated Quartz, BisGMA, Bisphenol A Dimethacrylate, 3M Unitek, Monrovia, CA, USA
Cercon xt ML Zirconium dioxide Dentsply Sirona, USA
e.max ZirCAD Yttrium-stabilized zirconium oxide Ivoclar Vivadent, USA
STML-ML Katana Zirconia Zirconium oxide, Yttrium oxide, Nickel oxide Kuraray Noritake, Japan

Shear bond strength.

Group N Obs Mean (MPa) Std Dev Coeff of Variation
Comparison (Enamel) 8 20.0 14.1 70.14
1A Cercon + Monobond 10 11.5 3.02 26.3
1B Cercon + ZPrime 10 9.24 3.50 37.91
Plus 2A ZirCAD + Monobond 10 11.6 4.06 35.03
2B ZirCAD + ZPrime Plus 10 11.4 4.48 39.27
3A Katana + Monobond 9 7.46 3.36 45.06
3B Katana + ZPrime Plus 8 8.34 1.99 23.87